Study on tempering behaviour of AISI 410 stainless steel AD Gopa Chakraborty, C.R. Das, S.K. Albert, A.K. Bhaduri, V. Thomas Paul, G ... Materials Characterization 100, 81-87, 2015 | 101 | 2015 |
Delta ferrite in the weld metal of reduced activation ferritic martensitic steel S Sam, CR Das, V Ramasubbu, SK Albert, AK Bhaduri, T Jayakumar, ... Journal of Nuclear Materials 455 (1-3), 343-348, 2014 | 91 | 2014 |
Study on microstructure and wear properties of different nickel base hardfacing alloys deposited on austenitic stainless steel G Chakraborty, N Kumar, CR Das, SK Albert, AK Bhaduri, S Dash, ... Surface and coatings technology 244, 180-188, 2014 | 76 | 2014 |
Selection of filler wire for and effect of auto tempering on the mechanical properties of dissimilar metal joint between 403 and 304L (N) stainless steels CR Das, AK Bhaduri, G Srinivasan, V Shankar, S Mathew Journal of materials processing technology 209 (3), 1428-1435, 2009 | 75 | 2009 |
Microstructural investigations on simulated intercritical heat-affected zone of boron modified P91-steel A Khajuria, M Akhtar, R Bedi, R Kumar, M Ghosh, CR Das, SK Albert Materials Science and Technology 36 (13), 1407-1418, 2020 | 69 | 2020 |
Effect of prior microstructure on microstructure and mechanical properties of modified 9Cr–1Mo steel weld joints CR Das, SK Albert, AK Bhaduri, G Srinivasan, BS Murty Materials Science and Engineering: A 477 (1-2), 185-192, 2008 | 65 | 2008 |
Finite element analysis of effect of triaxial state of stress on creep cavitation and rupture behaviour of 2.25 Cr–1Mo steel S Goyal, K Laha, CR Das, S Panneerselvi, MD Mathew International Journal of Mechanical Sciences 75, 233-243, 2013 | 62 | 2013 |
Scratch resistance and tribological properties of DLC coatings under dry and lubrication conditions N Sharma, N Kumar, S Dash, CR Das, RVS Rao, AK Tyagi, B Raj Tribology International 56, 129-140, 2012 | 62 | 2012 |
Influence of welding process on Type IV cracking behavior of P91 steel M Divya, CR Das, SK Albert, S Goyal, P Ganesh, R Kaul, J Swaminathan, ... Materials Science and Engineering: A 613, 148-158, 2014 | 61 | 2014 |
Finite element analysis of uniaxial and multiaxial state of stress on creep rupture behaviour of 2.25 Cr–1Mo steel S Goyal, K Laha, CR Das, SP Selvi, MD Mathew Materials Science and Engineering: A 563, 68-77, 2013 | 59 | 2013 |
Surface optical modes in GaN nanowires P Sahoo, S Dhara, S Dash, AK Tyagi, B Raj, CR Das, P Chandramohan, ... International journal of nanotechnology 7 (9-12), 823-832, 2010 | 56 | 2010 |
Weldability of 17-4PH stainless steel in overaged heat treated condition CR Das, HC Dey, G Srinivasan, SK Albert, AK Bhaduri, A Dasgupta Science and Technology of Welding and Joining 11 (5), 502-508, 2006 | 56 | 2006 |
Influence of boron on microstructure and mechanical properties of Gleeble simulated heat-affected zone in P91 steel A Khajuria, M Akhtar, R Bedi, R Kumar, M Ghosh, CR Das, SK Albert International Journal of Pressure Vessels and Piping 188, 104246, 2020 | 53 | 2020 |
A novel procedure for fabrication of wear-resistant bushes for high-temperature application CR Das, SK Albert, AK Bhaduri, G Kempulraj Journal of Materials Processing Technology 141 (1), 60-66, 2003 | 47 | 2003 |
Effect of constraint on creep behavior of 9Cr-1Mo steel S Goyal, K Laha, CR Das, S Panneerselvi, MD Mathew Metallurgical and Materials Transactions A 45, 619-632, 2014 | 44 | 2014 |
Transition of crack from Type IV to Type II resulting from improved utilization of Boron in the modified 9Cr-1Mo steel weldment CR Das, SK Albert, J Swaminathan, S Raju, AK Bhaduri, BS Murty Metallurgical and Materials Transactions A 43, 3724-3741, 2012 | 41 | 2012 |
Influence of the mode of laser welding parameters on microstructural morphology in thin sheet Ti6Al4V alloy B Kumar, S Bag, CP Paul, CR Das, R Ravikumar, KS Bindra Optics & Laser Technology 131, 106456, 2020 | 40 | 2020 |
Characterisation of nickel based hardfacing deposits on austenitic stainless steel CR Das, SK Albert, AK Bhaduri, C Sudha, ALE Terrance Surface engineering 21 (4), 290-296, 2005 | 39 | 2005 |
Improving 410NiMo weld metal toughness by PWHT M Divya, CR Das, V Ramasubbu, SK Albert, AK Bhaduri Journal of Materials Processing Technology 211 (12), 2032-2038, 2011 | 37 | 2011 |
Effects of dilution on microstructure and wear behaviour of NiCr hardface deposits CR Das, SK Albert, AK Bhaduri, R Nithya Materials Science and Technology 23 (7), 771-779, 2007 | 37 | 2007 |