Grain size dependence of hardness and fracture toughness in pure near fully-dense boron carbide ceramics BM Moshtaghioun, D Gomez-Garcia, A Dominguez-Rodriguez, RI Todd Journal of the European Ceramic Society 36 (7), 1829-1834, 2016 | 155 | 2016 |
Effect of spark plasma sintering parameters on microstructure and room-temperature hardness and toughness of fine-grained boron carbide (B4C) BM Moshtaghioun, FL Cumbrera-Hernández, D Gómez-García, ... Journal of the european ceramic society 33 (2), 361-369, 2013 | 148 | 2013 |
Toughening of super-hard ultra-fine grained B4C densified by spark-plasma sintering via SiC addition BM Moshtaghioun, AL Ortiz, D Gómez-García, A Domínguez-Rodríguez Journal of the european ceramic society 33 (8), 1395-1401, 2013 | 147 | 2013 |
Additive-free superhard B4C with ultrafine-grained dense microstructures BM Moshtaghioun, FL Cumbrera, AL Ortiz, M Castillo-Rodríguez, ... Journal of the European Ceramic Society 34 (3), 841-848, 2014 | 98 | 2014 |
Rapid carbothermic synthesis of silicon carbide nano powders by using microwave heating BM Moshtaghioun, R Poyato, FL Cumbrera, S de Bernardi-Martin, ... Journal of the european ceramic society 32 (8), 1787-1794, 2012 | 98 | 2012 |
Densification of B4C nanopowder with nanograin retention by spark-plasma sintering BM Moshtaghioun, AL Ortiz, D Gomez-Garcia, A Dominguez-Rodriguez Journal of the European Ceramic Society 35 (6), 1991-1998, 2015 | 73 | 2015 |
Spark plasma sintering of fine-grained alumina ceramics reinforced with alumina whiskers Y Tamura, BM Moshtaghioun, D Gomez-Garcia, AD Rodríguez Ceramics International 43 (1), 658-663, 2017 | 45 | 2017 |
Spark plasma sintering of titanium nitride in nitrogen: does it affect the sinterability and the mechanical properties? BM Moshtaghioun, D Gómez-García, A Domínguez-Rodríguez Journal of the European Ceramic Society 38 (4), 1190-1196, 2018 | 44 | 2018 |
High-temperature creep deformation of coarse-grained boron carbide ceramics BM Moshtaghioun, DG García, AD Rodríguez, NP Padture Journal of the European Ceramic Society 35 (5), 1423-1429, 2015 | 44 | 2015 |
A study on the effects of silica particle size and milling time on synthesis of silicon carbide nanoparticles by carbothermic reduction BM Moshtaghioun, A Monshi, MH Abbasi, F Karimzadeh International Journal of Refractory Metals and Hard Materials 29 (6), 645-650, 2011 | 41 | 2011 |
Abrasive wear rate of boron carbide ceramics: Influence of microstructural and mechanical aspects on their tribological response BM Moshtaghioun, D Gomez-Garcia, A Dominguez-Rodriguez, RI Todd Journal of the European Ceramic Society 36 (16), 3925-3928, 2016 | 39 | 2016 |
Graphene or carbon nanofiber-reinforced zirconia composites: Are they really worthwhile for structural applications? R Cano-Crespo, BM Moshtaghioun, D Gómez-García, R Moreno, ... Journal of the European Ceramic Society 38 (11), 3994-4002, 2018 | 34 | 2018 |
High-temperature deformation of fully-dense fine-grained boron carbide ceramics: Experimental facts and modeling BM Moshtaghioun, DG García, AD Rodríguez Materials & Design 88, 287-293, 2015 | 31 | 2015 |
High-temperature creep of carbon nanofiber-reinforced and graphene oxide-reinforced alumina composites sintered by spark plasma sintering R Cano-Crespo, BM Moshtaghioun, D Gómez-García, ... Ceramics International 43 (9), 7136-7141, 2017 | 28 | 2017 |
Enhancing the spark-plasma sinterability of B4C nanopowders via room-temperature methylation induced purification BM Moshtaghioun, D Gómez-García, A Domínguez-Rodríguez, AL Ortiz Journal of the European Ceramic Society 36 (11), 2843-2848, 2016 | 28 | 2016 |
High-temperature plastic deformation of spark plasma sintered boron carbide-based composites: The case study of B4C–SiC with/without graphite (g) BM Moshtaghioun, DG García, A Domínguez-Rodríguez Journal of the European Ceramic Society 36 (5), 1127-1134, 2016 | 28 | 2016 |
Carbon nanofibers replacing graphene oxide in ceramic composites as a reinforcing-phase: Is it feasible? R Cano-Crespo, BM Moshtaghioun, D Gómez-García, ... Journal of the European Ceramic Society 37 (12), 3791-3796, 2017 | 23 | 2017 |
Ceramics of Ta-doping stabilized orthorhombic ZrO2 densified by spark plasma sintering and the effect of post-annealing in air G Sponchia, BM Moshtaghioun, A Benedetti, P Riello, D Gómez-García, ... Scripta Materialia 130, 128-132, 2017 | 17 | 2017 |
Is an alumina-whisker-reinforced alumina composite the most efficient choice for an oxidation-resistant high-temperature ceramic? Y Tamura, BM Moshtaghioun, E Zapata-Solvas, D Gomez-Garcia, ... Journal of the European Ceramic Society 38 (4), 1812-1818, 2018 | 16 | 2018 |
Hot corrosion mechanism of tundish plaster with steel slags in continuous casting BM Moshtaghioun, A Monshi Journal of materials science 42, 6720-6728, 2007 | 16 | 2007 |