Urmăriți
Pavan A H V
Pavan A H V
Manager, Corporate R&D Division, BHEL, Hyderabad
Adresă de e-mail confirmată pe bhel.in
Titlu
Citat de
Citat de
Anul
Effect of laser peening and shot peening on fatigue striations during FCGR study of Ti6Al4V
BK Pant, AHV Pavan, RV Prakash, M Kamaraj
International Journal of Fatigue 93, 38-50, 2016
952016
Development and evaluation of SUS 304H—IN 617 welds for advanced ultra supercritical boiler applications
AHV Pavan, KSN Vikrant, R Ravibharath, K Singh
Materials Science and Engineering: A 642, 32-41, 2015
952015
Studies towards development of laser peening technology for martensitic stainless steel and titanium alloys for steam turbine applications
BK Pant, R Sundar, H Kumar, R Kaul, AHV Pavan, K Ranganathan, ...
Materials Science and Engineering: A 587, 352-358, 2013
722013
Root cause analysis of bowl-mill pinion shaft failures
AHV Pavan, KSN Vikrant, M Swamy, G Jayaraman
Case Studies in Engineering Failure Analysis 1 (2), 103-109, 2013
312013
Stress rupture embrittlement in cast Ni-based superalloy 625
AHV Pavan, RL Narayan, M Swamy, K Singh, U Ramamurty
Materials Science and Engineering: A 793, 139811, 2020
212020
Estimation of residual life of boiler tubes using steamside oxide scale thickness
KSN Vikrant, GV Ramareddy, AHV Pavan, K Singh
International journal of pressure vessels and piping 104, 69-75, 2013
192013
Effect of ageing on microstructure, mechanical properties and creep behavior of alloy 740H
AHV Pavan, RL Narayan, K Singh, U Ramamurty
Metallurgical and Materials Transactions A 51, 5169-5179, 2020
172020
Creep-rupture behavior of SUS 304H–IN 617 dissimilar metal welds for AUSC boiler applications
AHV Pavan, R Ravibharath, K Singh
Materials Science Forum 830, 199-202, 2015
172015
Mechanical behavior and dynamic strain ageing in Haynes® 282 superalloy subjected to accelerated ageing
AHV Pavan, RL Narayan, SH Li, K Singh, U Ramamurty
Materials Science and Engineering: A 832, 142486, 2022
132022
Hot corrosion studies on alloy 617 OCC in the context of its use in advanced ultra-supercritical (A-USC) power plants
PR Hari, N Arivazhagan, MN Rao, AHV Pavan
Transactions of the Indian Institute of Metals 70, 775-781, 2017
132017
Root cause analysis of steam turbine blade failure
MC Antony Harison, M Swamy, AHV Pavan, G Jayaraman
Transactions of the Indian Institute of Metals 69 (2), 659-663, 2016
132016
Creep modelling of P91 steel for high temperature power plant applications
S Nandi, KSN Vikrant, P Ahv, K Singh, RN Ghosh
Procedia Engineering 55, 751-755, 2013
122013
Application of bending creep for examining effect of service conditions on creep response of steel
F Hijazi, J Kar, AHV Pavan, K Singh, P Kumar, V Jayaram
Materials Science and Engineering: A 766, 138398, 2019
92019
High temperature corrosion of alloy 617 OCC at 700° C in simulated USC power plant environment
PR Hari, N Arivazhagan, MN Rao, AHV Pavan
Materials Research Express 6 (7), 076557, 2019
82019
Oxidation studies on nickel-base superalloy 617 OCC
PR Hari, N Arivazhagan, MN Rao, AHV Pavan
Materials Today: Proceedings 27, 2763-2767, 2020
72020
Metallurgical analysis of SA-106 Gr. B pipe failure during hot bending
AHV Pavan, KSN Vikrant, G Vimalan, K Singh
Case Studies in Engineering Failure Analysis 1 (2), 120-130, 2013
62013
Behaviour of alloy 617 OCC under hot corrosion conditions encountered in boilers in A-USC power plants
PR Hari, N Arivazhagan, M Nageswara Rao, AHV Pavan
Transactions of the Indian Institute of Metals 72, 1511-1514, 2019
52019
Microstructural characterization and mechanical properties of sand cast and investment cast alloy 625 for HP/IP casing applications for advanced fossil fired power plants
M Swamy, P Laxminarayana, AHV Pavan, MCA Harison, G Jayaraman, ...
Materials Today: Proceedings 5 (13), 27118-27122, 2018
52018
Comparative studies on corrosion of alloy 617 OCC at 700 C in air and simulated coal ash environments
PR Hari, N Arivazhagan, MN Rao, AHV Pavan
Materials Today: Proceedings 5 (5), 11452-11459, 2018
52018
Effect of stress-hold and strain-hold during Creep-Fatigue Interaction of alloy 617 M
BV Kalyan, AHV Pavan, BS Rao, N Narasaiah
Materials Today Communications 39, 108731, 2024
42024
Sistemul nu poate realiza operația în acest moment. Încercați din nou mai târziu.