[HTML][HTML] Structure design, fabrication, properties of laminated ceramics: A review
L Cheng, M Sun, F Ye, Y Bai, M Li, S Fan… - International Journal of …, 2018 - Elsevier
Various methods exist to improve the toughness and reduce the sensitivity to the defects in
ceramic materials; however, the bionic laminated ceramics are the most promising ones. In …
ceramic materials; however, the bionic laminated ceramics are the most promising ones. In …
Multilayered ceramic composites–a review
FD Minatto, P Milak, A De Noni… - … in Applied Ceramics, 2015 - journals.sagepub.com
With the aim of improving the toughness of ceramic materials, laminated composites have
been successfully developed since Clegg et al.(1990) inserted weak interfaces using very …
been successfully developed since Clegg et al.(1990) inserted weak interfaces using very …
3D printing of layered ceramic/carbon fiber composite with improved toughness
Strong and tough ceramic materials are required for many structural applications, however,
these properties tend to be mutually exclusive in many man-made ceramic materials …
these properties tend to be mutually exclusive in many man-made ceramic materials …
Tough and damage-tolerant monolithic zirconia ceramics with transformation-induced plasticity by grain-boundary segregation
Conventional ceria-stabilized tetragonal zirconia (Ce-TZP) with modest flexural strength has
rarely been used as compared to yttria-stabilized zirconia, even though it has excellent …
rarely been used as compared to yttria-stabilized zirconia, even though it has excellent …
High failure resistance layered ceramics using crack bifurcation and interface delamination as reinforcement mechanisms
R Bermejo, R Danzer - Engineering Fracture Mechanics, 2010 - Elsevier
Layered ceramics designed with weak interfaces favour interface delamination, while
laminates with strong interfaces show higher strength and enhanced mechanical reliability …
laminates with strong interfaces show higher strength and enhanced mechanical reliability …
[HTML][HTML] High-temperature fracture behaviour of layered alumina ceramics with textured microstructure
J Schlacher, Z Chlup, AK Hofer, R Bermejo - Journal of the European …, 2023 - Elsevier
Mimicking the damage tolerance of biological materials such as nacre has been realised in
textured layered alumina ceramics, showing improved reliability as well as fracture …
textured layered alumina ceramics, showing improved reliability as well as fracture …
Efficient multiscale strategy for toughening HfB2 ceramics: A heterogeneous ceramic–metal layered architecture
Y Bai, B Zhang, H Du, L Cheng - Journal of the American …, 2021 - Wiley Online Library
A multiscale structural design was innovatively adopted herein to increase the toughness of
monolithic HfB2 ceramics. SiC whiskers (SiCw) and graphene oxide (GO) were used as …
monolithic HfB2 ceramics. SiC whiskers (SiCw) and graphene oxide (GO) were used as …
Modeling effects of temperature, laminated structure, flaws and residual stress on fracture toughness of multilayered and particulate ceramic matrix composites
R Wang, S Zhou, W Li - Ceramics International, 2023 - Elsevier
Considering that the ceramic matrix composites are frequently used in high-temperature
applications, it is extremely important to analyze their fracture toughness at high …
applications, it is extremely important to analyze their fracture toughness at high …
Low (and negative) thermal expansion Al2TiO5 materials and Al2TiO5-3Al2O3. 2SiO2-ZrTiO4 composite materials. Processing, initial zircon proportion effect, and …
Abstract Aluminum titanate (Al 2 TiO 5) materials and aluminum titanate-mullite-zirconium
titanate (Al 2 TiO 5-3Al 2 O 3. 2SiO 2-ZrTiO 4) composite materials were successfully …
titanate (Al 2 TiO 5-3Al 2 O 3. 2SiO 2-ZrTiO 4) composite materials were successfully …
The fabrication and mechanical properties of SiC/ZrB2 laminated ceramic composite prepared by spark plasma sintering
Laminated SiC/ZrB2 ceramic was fabricated by roll-compaction and spark plasma sintering
at 1600° C. A maximum fracture toughness of 12.3±0.3 MPam1/2 was measured for the …