[HTML][HTML] Copper corrosion and biocorrosion events in premise plumbing

IT Vargas, DA Fischer, MA Alsina, JP Pavissich… - Materials, 2017 - mdpi.com
Corrosion of copper pipes may release high amounts of copper into the water, exceeding
the maximum concentration of copper for drinking water standards. Typically, the events with …

Corrosion Protection of Copper Using Al2O3, TiO2, ZnO, HfO2, and ZrO2 Atomic Layer Deposition

JS Daubert, GT Hill, HN Gotsch… - … applied materials & …, 2017 - ACS Publications
Atomic layer deposition (ALD) is a viable means to add corrosion protection to copper metal.
Ultrathin films of Al2O3, TiO2, ZnO, HfO2, and ZrO2 were deposited on copper metal using …

[HTML][HTML] Sources of and solutions to toxic metal and metalloid contamination in small rural drinking water systems: a rapid review

JW Tracy, A Guo, K Liang, J Bartram… - International journal of …, 2020 - mdpi.com
Exposure to toxic metals and metalloids (TMs) such as arsenic and lead at levels of concern
is associated with lifelong adverse health consequences. As exposure to TMs from paint …

Preparation of mussel-inspired perfluorinated polydopamine film on brass substrates: superhydrophobic and anti-corrosion application

N Cao, Y Miao, D Zhang, R Boukherroub, X Lin… - Progress in Organic …, 2018 - Elsevier
Inspired by the adhesive properties of protein of mussels, perfluorinated polydopamine
(fPDA) film on brass surface was obtained through spontaneous polymerization of dopamine …

Ultra-thin Al 2 O 3 films grown by atomic layer deposition for corrosion protection of copper

Z Chai, Y Liu, J Li, X Lu, D He - RSC Advances, 2014 - pubs.rsc.org
Ultra-thin Al2O3 films with thickness in the range of 4.5–29.4 nm were prepared on a copper
substrate by atomic layer deposition (ALD) at the temperature of 150° C to protect the …

Surface analysis of Cu coated with ALD Al2O3 and its corrosion protection enhancement in NaCl solution: EIS and polarization

HS Bahari, H Savaloni - Materials Research Express, 2019 - iopscience.iop.org
Al 2 O 3 was coated on copper substrates with a thickness of 62 nm at 473 K temperature
using atomic layer deposition method. The morphology of the produced samples was …

[HTML][HTML] Copper tube pitting in Santa Fe municipal water caused by microbial induced corrosion

TD Burleigh, CG Gierke, N Fredj, PJ Boston - Materials, 2014 - mdpi.com
Many copper water lines for municipal drinking water in Santa Fe, New Mexico USA, have
developed pinhole leaks. The pitting matches the description of Type I pitting of copper …

Homeowners' decision‐making in a premise plumbing failure–prone area

J Lee, E Kleczyk, DJ Bosch, AM Dietrich… - Journal‐American …, 2013 - Wiley Online Library
Two formal preference‐elicitation methodologies—conjoint analysis and the analytical
hierarchical process—were applied to examine the actions taken by homeowners living in a …

Copper pitting in chlorinated, high‐pH potable water

E Sarver, K Dodson, RP Scardina… - Journal‐American …, 2011 - Wiley Online Library
Copper pitting corrosion in potable water systems poses economic and environmental
problems associated with pinhole leaks. In the laboratory it has proven difficult to reproduce …

Copper pinhole failures: plumbing susceptibility and management

OE Farooqi, GV Loganathan, MA Edwards… - Journal of Water …, 2009 - ascelibrary.org
Consumers face numerous problems when they experience leaks and premature failures in