Recent progress in the development of SiC composites for nuclear fusion applications
Silicon carbide (SiC) fiber reinforced SiC matrix composites continue to undergo
development for fusion applications worldwide because of inherent advantages of the …
development for fusion applications worldwide because of inherent advantages of the …
Microstructure, mechanical property and bonding mechanism of SiC ceramic joint using a novel Y2Si2O7/Mullite glass-ceramic interlayer
L Sun, S Wang, C Hou, D Wang, C Liu, X Zhang… - Ceramics …, 2023 - Elsevier
Joining of SiC ceramics with a pre-oxidized or unoxidized surface and the subsequent
mechanical properties have been studied using Y 2 O 3–Al 2 O 3–SiO 2 glass bonding …
mechanical properties have been studied using Y 2 O 3–Al 2 O 3–SiO 2 glass bonding …
Effect of CaO do** on the properties and crystallization behavior of Y2O3–Al2O3–SiO2 glass
S Yang, Y Ma, J Li, S Kou, B Chen, C Liu, J Deng… - Ceramics …, 2023 - Elsevier
Abstract Nowadays, Y 2 O 3–Al 2 O 3–SiO 2 (YAS) glass joining is considered to be a
promising scheme for nuclear-grade continuous silicon carbide (SiC) fiber reinforced SiC …
promising scheme for nuclear-grade continuous silicon carbide (SiC) fiber reinforced SiC …
CaO-Al2O3 glass-ceramic as a joining material for SiC based components: a microstructural study of the effect of Si-ion irradiation
The aim of this work was to investigate and discuss the microstructure and interface reaction
of a calcia-alumina based glass-ceramic (CA) with SiC. CA has been used for several years …
of a calcia-alumina based glass-ceramic (CA) with SiC. CA has been used for several years …
[HTML][HTML] Helium bubbles in Gd2Ti2O7 borosilicate glass-ceramic composites
Glass-ceramics have the potential to be the advanced nuclear wasteforms that can
incorporate radioactive nuclides for a long-term geological disposal. In order to understand …
incorporate radioactive nuclides for a long-term geological disposal. In order to understand …
Wetting and joining of surface-oxidized SiC ceramic with calcium lithium aluminosilicate glass filler
J Fang, L Sun, S Guo, T Shan, Y Wen, C Liu… - Applied Surface …, 2021 - Elsevier
A novel strategy was developed to join SiC ceramics via a two-step method (ie, SiC surface
was modified by pre-oxidation treatment before bonding) using CaO-Li 2 O-Al 2 O 3-SiO 2 …
was modified by pre-oxidation treatment before bonding) using CaO-Li 2 O-Al 2 O 3-SiO 2 …
Study of helium swelling and embrittlement mechanisms in SiC ceramics
KM Tynyshbayeva, KK Kadyrzhanov, AL Kozlovskiy… - Crystals, 2022 - mdpi.com
This work is devoted to the study of the radiation damage kinetics and subsequent
embrittlement of the near-surface layer of SiC ceramics subjected to irradiation with low …
embrittlement of the near-surface layer of SiC ceramics subjected to irradiation with low …
Glass as a joining material for ceramic matrix composites: 25 years of research at Politecnico di Torino
A revision and update about the research activity done in the past 25 years at Politecnico di
Torino (Italy) on design and testing of glasses and glass‐ceramics for the joining of Ceramic …
Torino (Italy) on design and testing of glasses and glass‐ceramics for the joining of Ceramic …
Insights into grain boundary segregation and solubility limit of Cr in (TiZrNbTaCr) C
W Su, L Chen, W Zhang, S Huo, Y Wang… - Journal of Materials …, 2023 - Elsevier
Abstract Dense (TiZrNbTaCr) C with Cr segregation along grain boundaries (GBs) has been
first proposed and fabricated by pressureless sintering at 1800–2000° C, utilizing the self …
first proposed and fabricated by pressureless sintering at 1800–2000° C, utilizing the self …
[HTML][HTML] A yttrium aluminosilicate glass-ceramic to join SiC/SiC composites
In this work, a yttrium aluminosilicate glass-ceramic was employed to join two different
SiC/SiC ceramic matrix composites to be used as radiant tube furnace components for …
SiC/SiC ceramic matrix composites to be used as radiant tube furnace components for …