[HTML][HTML] Fatigue test setups and analysis methods for asphalt mixture: A state-of-the-art review
H Cheng, L Sun, Y Wang, L Liu, X Chen - Journal of Road Engineering, 2022 - Elsevier
Fatigue performance evaluation on asphalt mixture provides an essential reference for
asphalt mixture design and pavement structure design. Laboratory fatigue test has been …
asphalt mixture design and pavement structure design. Laboratory fatigue test has been …
[HTML][HTML] A review on evaluation of crack resistance of asphalt mixture by semi-circular bending test
Y Meng, W Kong, C Gou, S Deng, Y Hu, J Chen… - Journal of Road …, 2023 - Elsevier
Although there are many kinds of fracture tests to choose from in evaluating the crack
resistance of asphalt mixture, the semi-circular bending (SCB) test has attracted a lot of …
resistance of asphalt mixture, the semi-circular bending (SCB) test has attracted a lot of …
Validation of the favorable quantity of fly ash in concrete and analysis of crack propagation and its length–Using the crack tip tracking (CTT) method–In the fracture …
GL Golewski - Construction and Building Materials, 2021 - Elsevier
This article focuses on the analysis of fracture processes in fly ash (FA) concrete considering
the second model of cracking. The basic parameter of fracture mechanics in concrete …
the second model of cracking. The basic parameter of fracture mechanics in concrete …
Experimental investigation on the elastic modulus and fracture properties of basalt fiber–reinforced fly ash geopolymer concrete
Y Wang, S Hu, X Sun - Construction and Building Materials, 2022 - Elsevier
A comprehensive experimental study was conducted to explore the fracture characteristics
of basalt fiber–reinforced fly ash geopolymer concretes (FAGCs) with different fiber contents …
of basalt fiber–reinforced fly ash geopolymer concretes (FAGCs) with different fiber contents …
Studies of fracture toughness in concretes containing fly ash and silica fume in the first 28 days of curing
GL Golewski, DM Gil - Materials, 2021 - mdpi.com
This paper presents the results of the fracture toughness of concretes containing two mineral
additives. During the tests, the method of loading the specimens according to Mode I fracture …
additives. During the tests, the method of loading the specimens according to Mode I fracture …
Effects of specimen size and loading conditions on the fracture behaviour of asphalt concretes in the SCB test
The semi-circular bending (SCB) test has gained popularity for cracking evaluation of
asphalt concrete due to its simplicity in the test setup and sample preparation. The current …
asphalt concrete due to its simplicity in the test setup and sample preparation. The current …
Rubber modified high strength-high ductility concrete: Effect of rubber replacement ratio and fiber length
J Su, G Chen, H Pan, JX Lin, J Zhang, K Zhuo… - … and Building Materials, 2023 - Elsevier
High-strength high-ductility concrete (HSHDC) have gained significant attention due to its
high compressive strength and tensile ductility. However, the high fracture toughness of …
high compressive strength and tensile ductility. However, the high fracture toughness of …
Mixed mode-I/II fatigue performance of Cement Emulsified Asphalt Mortar: Experimental and statistical analysis at intermediate temperature
This study has investigated fatigue life of Cement Emulsified Asphalt Mortar (CEAM) under
mixed-mode I/II loadings at the intermediate temperature. For this investigation, SCB …
mixed-mode I/II loadings at the intermediate temperature. For this investigation, SCB …
A fracture-based approach to characterize long-term performance of asphalt mixes under moisture and freeze-thaw conditions
This study aims to quantify the fracture properties of asphalt mixes varying degrees of
moisture and freeze-thaw damages. The frequent occurrence of moisture and freeze-thaw …
moisture and freeze-thaw damages. The frequent occurrence of moisture and freeze-thaw …
Investigation of mode I fracture behavior of copper slag-SFRSCC
This study has examined how coarse CS (copper slag) aggregates (20–60%) and HESFs
(hooked-end steel fibers)(0.1–0.5%) affect the performance, microstructure, and …
(hooked-end steel fibers)(0.1–0.5%) affect the performance, microstructure, and …