Precipitation strengthening in nanostructured AZ31B magnesium thin films characterized by nano-indentation, STEM/EDS, HRTEM, and in situ TEM tensile testing

T Voisin, NM Krywopusk, F Mompiou, TP Weihs - Acta Materialia, 2017 - Elsevier
Abstract Thin magnesium (Mg) AZ31B (Mg-3Al-1Zn-< 0.4 Ca-< 0.3 Mn-< 0.2 Si in wt%) foils
were sputter deposited, aged, and mechanically tested at quasi-static strain rates. The as …

Effects of heat treatment on the wear behavior of surfacing AZ91 magnesium alloy

Q Chen, K Li, Y Liu, Z Zhao, K Tao… - Journal of Materials …, 2017 - cambridge.org
The surfacing welding has been widely utilized in the industrial equipment manufacturing
and repairs. The wear properties of surfacing alloys have an important effect on the whole …

Microhardness and microstructure characteristics of AZ91 magnesium alloy under different cooling rate conditions

AF Abd El-Rehim, HY Zahran… - Materials Research …, 2019 - iopscience.iop.org
The objective of the present work is to investigate the influence of aging time and cooling
rate conditions on the microstructure and mechanical properties of AZ91 magnesium alloy …

[HTML][HTML] Cerium addition improved the dry sliding wear resistance of surface welding AZ91 alloy

Q Chen, Z Zhao, Q Zhu, G Wang, K Tao - Materials, 2018 - mdpi.com
In this study, the effects of cerium (Ce) addition on the friction and wear properties of surface
welding AZ91 magnesium alloys were evaluated by pin-on-disk dry sliding friction and wear …