The relation between ductility and stacking fault energies in Mg and Mg–Y alloys
S Sandlöbes, M Friák, S Zaefferer, A Dick, S Yi… - Acta Materialia, 2012 - Elsevier
The underlying mechanisms that are responsible for the improved room-temperature
ductility in Mg–Y alloys compared to pure Mg are investigated by transmission electron …
ductility in Mg–Y alloys compared to pure Mg are investigated by transmission electron …
Effect of rare earth elements on the microstructure and texture development in magnesium–manganese alloys during extrusion
Single additions of the rare earth (RE) elements cerium, yttrium or neodymium have been
made to magnesium–manganese alloys in order to investigate their influence on the …
made to magnesium–manganese alloys in order to investigate their influence on the …
Tailoring the texture of magnesium alloy by twinning deformation to improve the rolling capability
Y **n, M Wang, Z Zeng, G Huang, Q Liu - Scripta Materialia, 2011 - Elsevier
A method to weaken the strong basal texture of rolled magnesium alloy by twinning
deformation is reported. Pre-rolling along the transverse direction at room temperature …
deformation is reported. Pre-rolling along the transverse direction at room temperature …
Effects of Ca and Sr additions on microstructure, mechanical properties, and ignition temperature of hot-rolled Mg–Zn alloy
In this study, the microstructures, mechanical properties, and ignition temperatures of hot-
rolled Mg-1.5 Zn-X (X: Ca and/or Sr) alloys were investigated. The Mg-1.5 Zn, Mg-1.5 Zn …
rolled Mg-1.5 Zn-X (X: Ca and/or Sr) alloys were investigated. The Mg-1.5 Zn, Mg-1.5 Zn …
Crystal plasticity-based forming limit prediction for non-cubic metals: application to Mg alloy AZ31B
CJ Neil, SR Agnew - International Journal of Plasticity, 2009 - Elsevier
A viscoplastic crystal plasticity model is incorporated within the Marciniak–Kuczynski (M–K)
approach for forming limit curve prediction. The approach allows for the incorporation of …
approach for forming limit curve prediction. The approach allows for the incorporation of …
An elasto-plastic constitutive model for evolving asymmetric/anisotropic hardening behavior of AZ31B and ZEK100 magnesium alloy sheets considering monotonic …
W Muhammad, M Mohammadi, J Kang… - International Journal of …, 2015 - Elsevier
Deformation twinning and texture evolution in hexagonal close-packed (HCP) metals lead to
evolving flow stress asymmetry/anisotropy and evolving plastic anisotropy. These …
evolving flow stress asymmetry/anisotropy and evolving plastic anisotropy. These …
Mg alloys: challenges and achievements in controlling performance, and future application perspectives
In recent years, Mg alloys have made inroads into applications for transport industries. The
favorable property profile of Mg promotes increased usage. Despite magnesium alloys …
favorable property profile of Mg promotes increased usage. Despite magnesium alloys …
Calcium and zirconium as texture modifiers during rolling and annealing of magnesium–zinc alloys
J Bohlen, J Wendt, M Nienaber, KU Kainer… - Materials …, 2015 - Elsevier
Rolling experiments were carried out on a ternary Mg–Zn–Ca alloy and its modification with
zirconium. Short time annealing of as-rolled sheets is used to reveal the microstructure and …
zirconium. Short time annealing of as-rolled sheets is used to reveal the microstructure and …
[HTML][HTML] Mechanical behavior of AZ31B Mg alloy sheets under monotonic and cyclic loadings at room and moderately elevated temperatures
NT Nguyen, OS Seo, CA Lee, MG Lee, J Kim, HY Kim - Materials, 2014 - mdpi.com
Large-strain monotonic and cyclic loading tests of AZ31B magnesium alloy sheets were
performed with a newly developed testing system, at different temperatures, ranging from …
performed with a newly developed testing system, at different temperatures, ranging from …
Role of yttrium in the microstructure and texture evolution of Mg
Single-phase solid solution alloys, Mg–2.9 Y and Mg–2.9 Zn (in wt%), and two-phase (α-Mg
solid solution+ intermetallic) Mg–Zn–Y alloys were deformed in uniaxial hot compression …
solid solution+ intermetallic) Mg–Zn–Y alloys were deformed in uniaxial hot compression …