Microstructure-property relationships of 420 stainless steel fabricated by laser-powder bed fusion

SD Nath, H Irrinki, G Gupta, M Kearns, O Gulsoy… - Powder Technology, 2019 - Elsevier
In this study, we report the mechanical properties, microstructure and corrosion behavior
99+% dense 420 stainless steel parts fabricated by laser-powder bed fusion (L-PBF). As …

Focused review on factors affecting martensitic stainless steels and super martensitic stainless steel passive film in the oil and gas field

S Malik, AB Radwan, N Al-Qahtani, A Abdullah… - Journal of Solid State …, 2024 - Springer
Martensitic and super martensitic stainless steels are widely used in the oil and gas industry
for general corrosion mitigation in the presence of sweet corrosion (CO2) and sour corrosion …

Adapting L-PBF process for fine powders: a case study in 420 stainless steel

SD Nath, A Okello, R Kelkar, G Gupta… - Materials and …, 2022 - Taylor & Francis
The laser-powder bed fusion (L-PBF), also known as selective laser melting (SLM), is widely
processed to a narrow powder size of 15 (D10) to 45 (D90) µm. However, expanding the …

[HTML][HTML] Effect of alloying elements on the sharpness retention of knife blades made of high carbon martensitic stainless steels

D Wu, Q Zhang, W Liu - Metals, 2022 - mdpi.com
Blades usually become blunt as the blade tip suffers wear during cutting, and improving the
sharpness retention of steel blades has become an attractive prospect in various industries …

Effect of Aging Treatment on Long-Term Salt Spray Corrosion Resistance of 15-5PH Stainless Steel

C Weng, J Tang, W Yu, Z Tang, R Qin - Metallurgical and Materials …, 2025 - Springer
The effects of aging treatment on the long-term salt spray corrosion resistance of 15-5PH
stainless steel were studied using white light interferometer, X-ray diffraction, X-ray …

Influence of parameters related to microstructure, chemical composition and environment characteristics on localized corrosion failure susceptibility of …

CVL Sabará, LNS Prachedes, LC Santos… - Engineering Failure …, 2021 - Elsevier
This work investigates the parameters that influence pitting resistance of UNS S41426
martensitic stainless steels. Chemical composition, microstructure, acceptable service …

Corrosion susceptibility behavior in 12Cr–1Mo martensitic stainless steel welded by SAW process and the effect of δ-ferrite in the HAZ

N Alcantar-Mondragón, F Reyes-Calderón… - International Journal of …, 2022 - Elsevier
Pitting corrosion in stainless steel (SS) is a punctual defect that promotes fatigue and cracks
propagation. Martensitic steel of steam turbine is exposed to the thermal cycle of welding …

Corrosion behavior of CA6NM in simulated geothermal brine highlighted by Electrochemical Impedance Spectroscopy (EIS)

A Nikitasari, E Mabruri, R Riastuti - Engineering and Applied …, 2021 - ph01.tci-thaijo.org
Martensitic stainless steel CA6NM has the potential to be utilized as a turbine blade material
for geothermal power plants because of its superior mechanical properties. However, the …

Pitting corrosion of 4Cr13 steel in a chlorine tank

Q Li, X **e, L **e, X **a, H Lou, W Pan… - Journal of Physics …, 2024 - iopscience.iop.org
Pitting corrosion is harmful and often occurs in chloride solution. The pitting corrosion of
4Cr13 steel in a chlorine tank was investigated in this study. Cr-depleted rings were …

[PDF][PDF] Effect of single and double tempering on corrosion behavior of modified CA6NM steel in 3.5% NaCl solution

M Rohmah, MS Anwar, I Astawa… - Int. J. Corros. Scale …, 2022 - researchgate.net
The modified Ca6NM cast martensitic stainless steel (MSS) was subjected to heat treatment
to explore the effect of tempering temperature and cycle on its corrosion behavior in a 3.5 …