[HTML][HTML] Measuring the interlaminar fracture toughness of thin carbon fiber/polyamide6 composites using adhesively bonded stiffeners
The present work investigates the interlaminar fracture toughness of a thin unidirectional
carbon fiber-reinforced/polyamide6 (CF/PA6) composite laminate. Aluminum (Al) stiffening …
carbon fiber-reinforced/polyamide6 (CF/PA6) composite laminate. Aluminum (Al) stiffening …
[HTML][HTML] Forming-behavior characterization of cross-ply carbon fiber/PA6 laminates using the bias-extension test
This work focuses on the in-plane shear behavior of carbon fiber-reinforced polyamide 6
cross-ply laminates. Bias-extension tests are performed at different temperatures and …
cross-ply laminates. Bias-extension tests are performed at different temperatures and …
Mode-I fracture toughness of thin CF/PA6 UD composites identified in a DCB test with stiffening Al beams in the presence of debonding
Compression molding of unidirectional (UD) carbon fiber-reinforced polyamide6 (CF/PA6)
prepreg tapes is conducted to manufacture thin 4-ply UD laminates. Two cooling rates of 43° …
prepreg tapes is conducted to manufacture thin 4-ply UD laminates. Two cooling rates of 43° …