Dual heterogeneous structures lead to ultrahigh strength and uniform ductility in a Co-Cr-Ni medium-entropy alloy
Alloys with ultra-high strength and sufficient ductility are highly desired for modern
engineering applications but difficult to develop. Here we report that, by a careful controlling …
engineering applications but difficult to develop. Here we report that, by a careful controlling …
Biocompatibility, osseointegration, antibacterial and mechanical properties of nanocrystalline Ti-Cu alloy as a new orthopedic material
The demands for high-performance biomaterials are driving the development of new
metallic alloys with improved mechanical and biological responses. In this study, a …
metallic alloys with improved mechanical and biological responses. In this study, a …
Allergy considerations in implanted neuromodulation devices
A Brown, NJ Mandelberg, D Munoz-Mendoza… - … : Technology at the …, 2021 - Elsevier
Objectives Allergic reactions are rare and poorly understood complications of
neuromodulation device implantation. There are currently no guidelines for management of …
neuromodulation device implantation. There are currently no guidelines for management of …
New Ti-Ta-Zr-Nb alloys with ultrahigh strength for potential orthopedic implant applications
In this study, a new series of Ti-Ta-Zr-Nb alloys (Ti-38.3 Ta-22Zr-8.1 Nb, Ti-38.9 Ta-25Zr-
5Nb, Ti-39.5 Ta-28Zr-2.5 Nb, designated TTZN-1, TTZN-2, TTZN-3, respectively) with high …
5Nb, Ti-39.5 Ta-28Zr-2.5 Nb, designated TTZN-1, TTZN-2, TTZN-3, respectively) with high …
Microstructure evolution and strengthening mechanisms of MP159 superalloy during room temperature rolling and cryorolling
WW Zhang, Y Yang, YB Tan, MT Zeng, M Ma… - Journal of Alloys and …, 2022 - Elsevier
Microstructure evolution and strengthening mechanisms of MP159 superalloy during room
temperature rolling (RTR) and cryorolling (CR) were studied by using the XRD, EBSD and …
temperature rolling (RTR) and cryorolling (CR) were studied by using the XRD, EBSD and …
[HTML][HTML] Annealing-induced hardening in single-phase FCC, equiatomic CrCoNi and non-equiatomic CrCoNiMo medium-entropy alloys
A two-step processing route including cold working (primary hardening) followed by
annealing-induced (secondary) hardening is proposed to strengthen single-phase face …
annealing-induced (secondary) hardening is proposed to strengthen single-phase face …
Revisiting MP35N and MP159: the route to ultra-strong Co–Cr–Ni medium entropy alloys
The recently emerged CoCrNi-based medium-entropy alloys (MEAs)/high-entropy alloys
(HEAs) have a good combination of high strength and ductility. However, there are still …
(HEAs) have a good combination of high strength and ductility. However, there are still …
Highly textured and twinned Cu films fabricated by pulsed electrodeposition
BZ Cui, K Han, Y **n, DR Waryoba, AL Mbaruku - Acta Materialia, 2007 - Elsevier
This paper reports the influence of substrates and peak current densities on: crystallographic
textures; twin density, thickness, spacing and twin boundary orientations; and electrical …
textures; twin density, thickness, spacing and twin boundary orientations; and electrical …
Investigation of secondary hardening in Co–35Ni–20Cr–10Mo alloy using analytical scanning transmission electron microscopy
D Sorensen, BQ Li, WW Gerberich, KA Mkhoyan - Acta Materialia, 2014 - Elsevier
The mechanism of secondary hardening in MP35N (Co–35Ni–20Cr–10Mo) alloy due to
exposures at elevated temperatures has been studied. It was observed that short exposure …
exposures at elevated temperatures has been studied. It was observed that short exposure …
Grain refinement of CoNiCrMo non-equiatomic medium entropy alloy
M Rezayat, F Najib - Metals and Materials International, 2023 - Springer
Using a thermal–mechanical process, the average grain size of Co35Ni34Cr24Mo7 medium
entropy alloy was reduced to 2 μm, resulted in 50% improvement of hardness. In this way …