Effect of porosity morphology and elements characteristics on mechanical property in T-joints during dual laser-beam bilateral synchronous welding of 2060/2099 Al …
D Chen, X Zhan, T Liu, Y Zhao, N Qi, L Sun - Optics & Laser Technology, 2021 - Elsevier
Abstract The 2 mm thick 2060-T8/2099-T83 Al-Li alloy T-joints were welded by dual laser-
beam bilateral synchronous welding (DLBSW) with ER4047 filler wire. The metallurgical …
beam bilateral synchronous welding (DLBSW) with ER4047 filler wire. The metallurgical …
TSA anodising voltage effects on the near-surface coarse intermetallic particles in the AA2024-T3 and AA2198-T8 alloys
JV de Sousa Araujo, M Xavier Milagre… - Corrosion …, 2022 - Taylor & Francis
In this study, the behaviour of the micrometric particles of the AA2198-T8 alloy during
anodising at various voltages and the effect of anodising voltage on the anodised surface …
anodising at various voltages and the effect of anodising voltage on the anodised surface …
Corrosion behavior of 2198 Al–Cu–Li alloy in different aging stages in 3.5 wt% NaCl aqueous solution
Y Zou, X Chen, B Chen - Journal of Materials Research, 2018 - cambridge.org
In this paper, corrosion behavior of 2198 Al–Cu–Li alloy in different aging stages is
investigated using immersion and electrochemical measurements in 3.5 wt% NaCl aqueous …
investigated using immersion and electrochemical measurements in 3.5 wt% NaCl aqueous …
[HTML][HTML] Synergistic enhancement of Ag layer and Cu particles on SERS property of spontaneously formed Cu nanoparticles/Ta–Cu alloy thin films
S Li, S Liang, H Zhang, P Shi, M Shen, H Zheng… - Journal of Materials …, 2023 - Elsevier
Surface-enhanced Raman scattering (SERS) is a highly accurate and ultra-sensitive single-
molecule detection technology. Ta–Cu alloy thin films were prepared by co-sputtering …
molecule detection technology. Ta–Cu alloy thin films were prepared by co-sputtering …
An examination of the composition and microstructure of coarse intermetallic particles in AA2099-T8, including Li detection
Electron and proton microprobes, along with electron backscatter diffraction (EBSD) analysis
were used to study the microstructure of the contemporary Al–Cu–Li alloy AA2099-T8. In …
were used to study the microstructure of the contemporary Al–Cu–Li alloy AA2099-T8. In …
Artificial neural network modeling to evaluate the dynamic flow stress of 7050 aluminum alloy
G Quan, T Wang, Y Li, Z Zhan, Y **a - Journal of Materials Engineering …, 2016 - Springer
The flow stress data have been obtained by a set of isothermal hot compression tests, which
were carried out in the temperature range of 573-723 K and strain rates of 0.01, 0.1, 1, and …
were carried out in the temperature range of 573-723 K and strain rates of 0.01, 0.1, 1, and …
[HTML][HTML] The influence of Zn addition on microstructure of an Al-1.7 Cu-4.0 Li-0.4 Mg alloy
D Liu, Y Ma, J Li, C Huang, Y Wang, Z Wang… - Journal of Materials …, 2020 - Elsevier
The tensile properties and corrosion behaviours of an ageing Al-1.7 Cu-4.0 Li-0.4 Mg alloys
(in at.%) with or without 0.3 Zn addition were investigated by detailed microstructure …
(in at.%) with or without 0.3 Zn addition were investigated by detailed microstructure …
Evolution of micropores and second phases during hot deformation of 2050 Al-Li alloy
R Luo, Z Zhou, X Ma, Y Xu, Y Cai, X Hou… - Journal of Alloys and …, 2024 - Elsevier
Microporosity and second phases are typical components for casting 2050 alloy. In this
paper, the evolution of both microporosity and the second phases during hot deformation of …
paper, the evolution of both microporosity and the second phases during hot deformation of …
Observations on the early stages of corrosion on AA2099-T83
Abstract An Al–Cu–Li aerospace alloy has been investigated to determine the order in which
corrosion at different types of sites occurs in AA2099-T83. Specifically, the sequence of …
corrosion at different types of sites occurs in AA2099-T83. Specifically, the sequence of …
Localised corrosion of intermetallic particles on aluminium AA2099-T8
F Peltier, D Thierry - Corrosion Engineering, Science and …, 2021 - journals.sagepub.com
Specimens of AA2099-T8 were immersed for different times ranging from 2 to 180 min in 0.1
M NaCl. The development of corrosion around intermetallic particles was studied by …