Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam
The microstructure and microchemistry of the oxide scales formed on Fe-21Cr-32Ni and Fe-
17Cr-9Ni steels after exposure to deaerated high-temperature high-pressure steam at 600° …
17Cr-9Ni steels after exposure to deaerated high-temperature high-pressure steam at 600° …
Short-term oxidation behavior of 304 stainless steel in N2-21 vol% O2 environment between 900 and 1200° C
M Su, J Zhao, Z Tian, C Gu - Corrosion Science, 2022 - Elsevier
Oxidation behavior and microstructure evolution of 304 stainless steel at 900–1200° C in N
2-21 vol% O 2 were investigated. At 900° C, Cr 2 O 3 protective oxide is formed on the …
2-21 vol% O 2 were investigated. At 900° C, Cr 2 O 3 protective oxide is formed on the …
TEM comparative study on oxide films of 316L and T91 steel exposed to 350–500° C steam
C Liu, L Qi, T Shen, P **, Z Wang - Journal of Materials Science & …, 2024 - Elsevier
The oxide films of 316L and T91 exposed to 350–500° C steam were investigated using
transmission electron microscopy (TEM). Independent of the exposure temperature, a triplex …
transmission electron microscopy (TEM). Independent of the exposure temperature, a triplex …
Oxidation behavior of the directed energy deposited 316L stainless steel in supercritical carbon dioxide environment: Effect of post-manufacturing heat treatment
The oxidation behaviors of directed energy deposit (DED) 316L SS with various post-DED
heat treatments (HTs) as well as commercial 316L SS were investigated in a 650℃/20 MPa …
heat treatments (HTs) as well as commercial 316L SS were investigated in a 650℃/20 MPa …
[HTML][HTML] Experimental study on steam oxidation resistance at 600° C of Inconel 625 coatings deposited by HVOF and laser cladding
Abstract Inconel 625 (IN625) coatings were deposited by High-Velocity Oxy-fuel (HVOF) and
laser cladding, on a 10.50–12% Cr steel to improve its oxidation resistance. Both as …
laser cladding, on a 10.50–12% Cr steel to improve its oxidation resistance. Both as …
Corrosion behaviour of alumina-forming heat resistant alloy with Ti in high temperature steam
The corrosion behaviour of an alumina-forming heat resistant alloy with high Ti (Fe-35Ni-
16Cr-4.5 Al-3Ti, wt%) was evaluated in high temperature steam. The alloy developed …
16Cr-4.5 Al-3Ti, wt%) was evaluated in high temperature steam. The alloy developed …
[HTML][HTML] Improving the high-temperature oxidation resistance of Fe-18Cr-8Ni austenitic stainless steel by cold-rolling treatments
M Su, J Zhao, Z Tian, C Gu, Y Wang - Journal of Materials Research and …, 2022 - Elsevier
The effect of different degrees of cold rolling on the short-term oxidation behavior of Fe-18Cr-
8Ni stainless steel oxidized at 1000° C in N 2-21 vol% O 2 for 3 h was investigated. The …
8Ni stainless steel oxidized at 1000° C in N 2-21 vol% O 2 for 3 h was investigated. The …
Effects of surface treatments and temperature on the oxidation behavior of 308L stainless steel cladding in hydrogenated high-temperature water
T Cui, X Xu, D Pan, J Ma, Z Lu, J Chen, X Liang… - Journal of Nuclear …, 2022 - Elsevier
The properties of the oxide films grown on 308 L SS cladding with various surface
treatments and temperatures in simulated PWR primary water are studied. The thickness of …
treatments and temperatures in simulated PWR primary water are studied. The thickness of …
Microstructure and Hot Oxidation Resistance of Wrought and Wire Arc Additive Manufactured Austenitic Stainless Steel 347
A Rajesh Kannan, V Rajkumar… - steel research … - Wiley Online Library
Boiler steels in gas turbines and waste‐to‐energy recovery units undergo severe damage
due to oxidation. The hot oxidation behavior of wire arc additive manufactured austenitic …
due to oxidation. The hot oxidation behavior of wire arc additive manufactured austenitic …
Experimental study on steam oxidation resistance at 600° C of Inconel 625 coatings deposited by HVOF and laser cladding
A Illana Sánchez, MT Miguel Gamo, G García Martín… - 2022 - docta.ucm.es
ABSTRACT Inconel 625 (IN625) coatings were deposited by High-Velocity Oxy-fuel (HVOF)
and laser cladding, on a 10.50–12% Cr steel to improve its oxidation resistance. Both as …
and laser cladding, on a 10.50–12% Cr steel to improve its oxidation resistance. Both as …