Microstructure and wear behaviors of laser cladding in-situ synthetic (TiBx+ TiC)/(Ti2Ni+ TiNi) gradient composite coatings

J Liang, X Yin, Z Lin, S Chen, C Liu, C Wang - Vacuum, 2020 - Elsevier
Abstract TiNi/Ti 2 Ni-based gradient composite coatings reinforced with TiC and TiB x were
produced on TC4 substrates by laser cladding with different composition powder mixture …

Sliding wear of selective laser melting processed Ti6Al4V under boundary lubrication conditions

Y Zhu, X Chen, J Zou, H Yang - Wear, 2016 - Elsevier
Abstract The titanium alloy Ti 6 Al 4 V is widely used in industry due to its high strength-to-
mass ratio and good performance at high temperature. However, it exhibits poor tribological …

Influence of thermal oxidation duration on the microstructure and fretting wear behavior of Ti6Al4V alloy

S Wang, Z Liao, Y Liu, W Liu - Materials Chemistry and Physics, 2015 - Elsevier
Thermal oxidation under water oxidizing atmosphere was performed on Ti6Al4V alloy under
different durations from 2 h to 8 h. Surface characterizations were performed using X-ray …

Nano-and micro-tribological behaviours of plasma nitrided Ti6Al4V alloys

A Samanta, M Bhattacharya, I Ratha… - Journal of the …, 2018 - Elsevier
Plasma nitriding of the Ti-6Al-4V alloy (TA) sample was carried out in a plasma reactor with
a hot wall vacuum chamber. For ease of comparison these plasma nitrided samples were …

Wear and corrosion properties of a B–Al composite layer on pure titanium

X Wang, D Qu, Y Duan, M Peng - Ceramics International, 2022 - Elsevier
A boriding and aluminizing two-step method was used to fabricate a B–Al composite layer
on the surface of pure titanium. The composite layer was characterized by scanning electron …

Effect of different surface oxidation treatments on structural, mechanical and tribological properties of ultrafine-grained titanium

İ Çelik, A Alsaran, G Purcek - Surface and Coatings Technology, 2014 - Elsevier
Four different surface oxidation treatments, so-called, anodizing oxidation (AO), micro-arc
oxidation (MAO), plasma oxidation (PO) and thermal oxidation (TO), were applied to ultrafine …

Thermal oxidation of medical Ti6Al4V blasted with ceramic particles: Effects on the microstructure, residual stresses and mechanical properties

M Lieblich, S Barriuso, M Multigner… - Journal of the …, 2016 - Elsevier
Abstract Roughening of Ti6Al4V by blasting with alumina or zirconia particles improves the
mechanical fixation of implants by increasing the surface area available for bone/implant …

[HTML][HTML] On the improvement of AA2024 wear properties through the deposition of a cold-sprayed titanium coating

A Astarita, F Rubino, P Carlone, A Ruggiero, C Leone… - Metals, 2016 - mdpi.com
This paper deals with the study of the enhancement of the tribological properties of AA2024
through the deposition of a titanium coating. In particular two different coatings were …

The effect of plasma nitriding on the fatigue behavior of the Ti-6Al-4V alloy

MCB de Castro, AA Couto, GFC Almeida, M Massi… - Materials, 2019 - mdpi.com
The Ti-6Al-4V alloy is widely used in the manufacture of components that must have low
density and high corrosion resistance and fatigue strength. The fatigue strength can be …

Triode plasma diffusion treatment of titanium alloys

G Cassar, A Matthews, A Leyland - Surface and Coatings Technology, 2012 - Elsevier
In this paper the structure, properties and tribological behaviour of the binary β titanium alloy