Fracture toughness and structural evolution in the TiAlN system upon annealing
Hard coatings used to protect engineering components from external loads and harsh
environments should ideally be strong and tough. Here we study the fracture toughness, K …
environments should ideally be strong and tough. Here we study the fracture toughness, K …
[HTML][HTML] Fracture properties of thin film TiN at elevated temperatures
J Buchinger, L Löfler, J Ast, A Wagner, Z Chen… - Materials & …, 2020 - Elsevier
We provide an experimental and theoretical description of the high temperature fracture
behaviour of TiN thin films. For this, we employ molecular dynamics and density functional …
behaviour of TiN thin films. For this, we employ molecular dynamics and density functional …
Evaluation of the optimal Y content for the FeCrAl coating with excellent LBE corrosion resistance
W Zhang, Y Zhong, J Deng, M Zhou, R Wang… - Journal of Nuclear …, 2024 - Elsevier
FeCrAlY coating with excellent LBE corrosion resistance is considered one of the most
important candidate corrosion-resistant coatings in LFRs. However, the critical Y content …
important candidate corrosion-resistant coatings in LFRs. However, the critical Y content …
Reactive HiPIMS deposition of Ti-Al-N: Influence of the deposition parameters on the cubic to hexagonal phase transition
Reactive high-power impulse magnetron sputtering (R-HiPIMS) is seen as a key-technology
for the deposition of future hard and multifunctional coatings. Increased ionisation rates …
for the deposition of future hard and multifunctional coatings. Increased ionisation rates …
A comparative study on the structure and properties of TiAlSiN coatings deposited by FCVA and HiPIMS
Z Yin, S Wu, Y Zhang, W Yan, S Dai, X Peng… - Journal of Alloys and …, 2024 - Elsevier
The TiAlSiN coating has garnered significant interest due to its exceptional hardness, high
oxidation resistance temperature, robust film-substrate bond strength, excellent wear …
oxidation resistance temperature, robust film-substrate bond strength, excellent wear …
[HTML][HTML] Influence of Ta on the oxidation resistance of WB2− z coatings
C Fuger, B Schwartz, T Wojcik, V Moraes… - Journal of Alloys and …, 2021 - Elsevier
Ternary W 1− x Ta x B 2− z is a promising protective coating material possessing enhanced
ductile character and phase stability compared to closely related binaries. Here, the …
ductile character and phase stability compared to closely related binaries. Here, the …
[HTML][HTML] High-temperature oxidation resistance of NiAl intermetallic formed in situ by thermal spraying
Q Jia, D Li, S Li, Z Zhang, N Zhang - Coatings, 2018 - mdpi.com
An Al/Ni composite coating was deposited on the surface of a pure Ti substrate by arc spray
technology and plasma spray technology. In order to enable the in-situ reaction between the …
technology and plasma spray technology. In order to enable the in-situ reaction between the …
Impurity dominated thin film growth
FG Cougnon, A Dulmaa, R Dedoncker… - Applied Physics …, 2018 - pubs.aip.org
Magnetron sputter deposition was applied to grow thin metal films in the presence of
impurities. These impurities are ambient gas molecules and/or atoms from the residual gas …
impurities. These impurities are ambient gas molecules and/or atoms from the residual gas …
[HTML][HTML] Oxidation mechanism of sputter deposited model SiNx/TiN/SiNx coatings
TiSiN coatings are of high interest for the cutting industry, since they not only offer excellent
mechanical properties, but also exhibit exceptional oxidation resistance. Although up to date …
mechanical properties, but also exhibit exceptional oxidation resistance. Although up to date …
[HTML][HTML] Perspective on pathways towards responsible surface engineering
In this perspective sustainability-relevant aspects of modern surface engineering
technologies, which enable improved structural and functional surface properties, are …
technologies, which enable improved structural and functional surface properties, are …