Materials requirements in fused filament fabrication: a framework for the design of next‐generation 3D printable thermoplastics and composites
A Sola - Macromolecular Materials and Engineering, 2022 - Wiley Online Library
Fused filament fabrication (FFF), also known as fused deposition modeling, is the leading
technology for polymer‐based additive manufacturing. The simplicity, along with the …
technology for polymer‐based additive manufacturing. The simplicity, along with the …
Hygromechanical properties of 3D printed continuous carbon and glass fibre reinforced polyamide composite for outdoor structural applications
G Chabaud, M Castro, C Denoual, A Le Duigou - Additive Manufacturing, 2019 - Elsevier
The additive manufacturing of structural composites is a disruptive technology currently
limited by its moderate mechanical properties. Continuous fibre reinforcements have …
limited by its moderate mechanical properties. Continuous fibre reinforcements have …
Settling velocities of small microplastic fragments and fibers
S Dittmar, AS Ruhl, K Altmann… - Environmental Science & …, 2024 - ACS Publications
There is only sparse empirical data on the settling velocity of small, nonbuoyant
microplastics thus far, although it is an important parameter governing their vertical transport …
microplastics thus far, although it is an important parameter governing their vertical transport …
[HTML][HTML] Effect of molecular weight and hydration on the tensile properties of polyamide 12
Abstract Polyamide 12 (PA12) has found significant applications in the medical device
industry, including its common use as an outer jacket layer in catheters. Like all polymers …
industry, including its common use as an outer jacket layer in catheters. Like all polymers …
Evidence of small microplastics (< 100 μm) ingestion by Pacific oysters (Crassostrea gigas): A novel method of extraction, purification, and analysis using Micro-FTIR
Microplastics (MPs) are present in fresh, brackish, or marine waters. Micro-and
macroinvertebrates can mistake MPs or small microplastics (SMPs,< 100 μm) to be food …
macroinvertebrates can mistake MPs or small microplastics (SMPs,< 100 μm) to be food …
Prediction of mechanical behaviour of a bulk epoxy adhesive in a marine environment
A Ilioni, PY Le Gac, C Badulescu… - The Journal of …, 2019 - Taylor & Francis
This article describes an approach to predict the behaviour of an epoxy adhesive in bulk
form in a marine environment. First, the material, the experimental conditions and the …
form in a marine environment. First, the material, the experimental conditions and the …
Additives, plasticizers, small microplastics (< 100 μm), and other microlitter components in the gastrointestinal tract of commercial teleost fish: Method of extraction …
One of the aims of this study is the development of a pretreatment method for additives,
plasticizers and other components of micro-litter (APFs), and small microplastics (SMPs< …
plasticizers and other components of micro-litter (APFs), and small microplastics (SMPs< …
Yield stress changes induced by water in polyamide 6: Characterization and modeling
This paper considers the effect of water content on mechanical properties of polyamide 6
when used in a humid environment. First an experimental section presents the tensile …
when used in a humid environment. First an experimental section presents the tensile …
Modelling the non Fickian water absorption in polyamide 6
This paper investigates the water absorption of polyamide 6. The high amount of absorbed
water in the polymer and the large resulting decrease in the glass transition temperature (T …
water in the polymer and the large resulting decrease in the glass transition temperature (T …
Origin of embrittlement in Polyamide 6 induced by chemical degradations: Mechanisms and governing factors
Q Deshoulles, M Le Gall, C Dreanno, M Arhant… - Polymer Degradation …, 2021 - Elsevier
Polyamide 6 films were aged aged in two environments inducing either only oxidation or
only hydrolysis of the polymer for up to two years. Ageing temperatures ranged from 80° C to …
only hydrolysis of the polymer for up to two years. Ageing temperatures ranged from 80° C to …