Influence of chromium on the flow-accelerated corrosion behavior of low alloy steels in 3.5% NaCl solution
S Jiang, F Chai, H Su, C Yang - Corrosion Science, 2017 - Elsevier
The corrosion behavior of carbon steel and Cr-containing steels was investigated during
flow-accelerated corrosion. The corresponding weight loss and electrochemical properties …
flow-accelerated corrosion. The corresponding weight loss and electrochemical properties …
Flow accelerated corrosion rate on carbon steel pipe bend by thin layer activation technique and computational modeling: Under PHWR operating conditions
P Madasamy, P Chandramohan, M Mukunthan… - Engineering Failure …, 2021 - Elsevier
Carbon Steel (CS) pi** plays a vital role in the heat transport circuits of power plants.
These pipes undergo excessive degradation in some of the specific locations due to the flow …
These pipes undergo excessive degradation in some of the specific locations due to the flow …
On-Line Measurement and Characterization of Electrochemical Corrosion of 304L Stainless Steel Pipe Wall in High-Speed Cl-Containing Solution
J Cheng, Q Yan, Z Pan, W Wei - Metals, 2022 - mdpi.com
Fluid-induced metal corrosion failure is one of the main causes of pipe wall damage. In this
paper, aimed at the corrosion failure of stainless-steel pipe wall in high-speed flowing liquid …
paper, aimed at the corrosion failure of stainless-steel pipe wall in high-speed flowing liquid …
[PDF][PDF] Measurement of Seawater Flow-Induced Erosion Rates for Iron Surfaces using Thin Layer Activation Technique.
The laboratory-scale erosion-corrosion testing facility at BATAN's Center for Radioisotope
and Radiopharmaceutical Technology (PTRR) in Serpong was employed to simulate flow …
and Radiopharmaceutical Technology (PTRR) in Serpong was employed to simulate flow …
Enhancement of corrosion resistance in carbon steels using nickel-phosphorous/titanium dioxide nanocomposite coatings under high-temperature flowing water
To mitigate the corrosion of carbon steels in high-temperature flowing water, we deposited
Ni-P/TiO 2 nanocomposite coatings, composed of a Ni-P alloy matrix with dispersed TiO 2 …
Ni-P/TiO 2 nanocomposite coatings, composed of a Ni-P alloy matrix with dispersed TiO 2 …
Chemical dissolution of oxide layer on carbon steel SA 106 GR. B-based oxalic acid
The feeder pipes of the primary cooling system in a pressurized heavy water reactor
(PHWR) are composed of carbon steel SA 106 GR. B. On the surface of this structural …
(PHWR) are composed of carbon steel SA 106 GR. B. On the surface of this structural …
Effect of cathodic polarisation on the corrosion behaviour of 316L stainless steel under static and dynamic conditions
F Arjmand, A Adriaens - Corrosion Reviews, 2015 - degruyter.com
The role of cathodic polarisation on the corrosion of 316L stainless steel was investigated
under static and dynamic conditions. The results reveal that the applied flow regime during …
under static and dynamic conditions. The results reveal that the applied flow regime during …
Corrosion rate of carbon steel and aluminum alloy in sulfuric acid and hydrochloric acid solutions accelerated by microwave heating
Y Wang, D Wang, H Zhang - Asia‐Pacific Journal of Chemical …, 2013 - Wiley Online Library
Corrosion behavior of carbon steel and aluminum alloy in hydrochloric acid and sulfuric acid
solutions was studied using microwave heating and conventional water bath heating …
solutions was studied using microwave heating and conventional water bath heating …
Effect Of Mig Welding Process Parameters On Erosion And Corrosion Behavior Of Astm A106 Grade-B Pipe Weldments
Evaluating the integrity of the welded pipes used for fluid transportation in processing
industries demands certain investigations on the erosion and corrosion behavior under …
industries demands certain investigations on the erosion and corrosion behavior under …
[PDF][PDF] Novel Technologies for Mitigation of Flow Accelerated Corrosion of the Secondary Side of Pressurized Water Reactors
S Kim - 2019 - core.ac.uk
Secondary side of pressurized water reactors undergo severe erosion-corrosion (EC) under
high-temperature flowing water, and one of the most damaging phenomenon is flow …
high-temperature flowing water, and one of the most damaging phenomenon is flow …