[HTML][HTML] Friction stir welding/processing of metals and alloys: A comprehensive review on microstructural evolution

A Heidarzadeh, S Mironov, R Kaibyshev, G Çam… - Progress in Materials …, 2021 - Elsevier
The unique combination of very large strains, high temperatures and high strain rates
inherent to friction stir welding (FSW) and friction stir processing (FSP) and their dependency …

Study of the microstructure and mechanical performance of CX stainless steel processed by selective laser melting (SLM)

X Yan, C Chen, C Chang, D Dong, R Zhao… - Materials Science and …, 2020 - Elsevier
In this study, a new precipitation hardening stainless steel (PHSS), CX stainless steel, was
manufactured using selective laser melting (SLM) technology. Following SLM fabrication, a …

Deformation behavior and microstructure evolution during hot working of a coarse-grained Ti-5Al-5Mo-5V-3Cr-1Zr titanium alloy in beta phase field

XG Fan, Y Zhang, PF Gao, ZN Lei, M Zhan - Materials Science and …, 2017 - Elsevier
Isothermal compression of a coarse-grained Ti-55531 titanium alloy was carried out in the β
phase region to investigate the hot formability and microstructure evolution of the material. It …

Effect of chromium content on the corrosion resistance of ferritic stainless steels in sulfuric acid solution

Y Yu, S Shironita, K Souma, M Umeda - Heliyon, 2018 - cell.com
Due to recent increases in the price of Ni, steel use is currently undergoing a global shift
from austenitic stainless steels to ferritic stainless steels. In this study, the corrosion behavior …

Comparison of a copper processed by asymmetric unidirectional rolling (AUR) and cross rolling (ACR): Strain distribution, microstructure, texture, and mechanical …

H Solouki, R Jamaati, HJ Aval - Materials Chemistry and Physics, 2024 - Elsevier
In this work, the effect of strain path on the strain distribution, microstructural evolution,
crystallographic texture, and mechanical behavior of electrolytic tough-pitch copper was …

Constrained groove pressing and subsequent annealing of Al-Mn-Si alloy: microstructure evolutions, crystallographic transformations, mechanical properties …

H Pouraliakbar, MR Jandaghi, G Khalaj - Materials & Design, 2017 - Elsevier
Abstract Al-Mn-Si specimens were severe plastic deformed (SPDed) through constrained
groove pressing (CGP) by ε eff= 1.16, 232, and 3.48. CGPed sheets were subsequently …

Heterogeneous microstructure and deformation behavior of an automotive grade aluminum alloy

SS Dash, DJ Li, XQ Zeng, DL Chen - Journal of Alloys and Compounds, 2021 - Elsevier
Aluminum alloy is today considered as a prime selection for manufacturing lightweight
structural components in the automotive industry to increase fuel efficiency and reduce …

[HTML][HTML] Form-stable phase change materials with enhanced thermal stability and fire resistance via the incorporation of phosphorus and silicon

Y Jiang, P Yan, Y Wang, C Zhou, J Lei - Materials & Design, 2018 - Elsevier
In this paper, a series of novel form-stable phase change materials (PCMs) containing
phosphorus and silica were prepared by transesterification of diethyl phosphite with 1 …

Dissimilar friction stir welding of AA2198 and AA7475: Effect of solution treatment and aging on the microstructure and mechanical strength

MR Jandaghi, C Badini, M Pavese - Journal of Manufacturing Processes, 2020 - Elsevier
A post-weld heat treatment consisting of solution treatment and subsequent aging (STA) is
widely applied to aluminum joints fabricated by friction stir welding (FSW) to improve the …

Influence of effective strain on the corrosion behavior of nickel-based GH4710 superalloy in chloride solutions

F Sui, T An, S Zheng, L Chen, S Li - Corrosion Science, 2022 - Elsevier
The influence of effective strains with a range from 1.1 to 2 on the corrosion resistance of
GH4710 superalloy in chloride solutions was studied by potentiodynamic polarization …