Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: A review
The essential work of fracture (EWF) concept has become very popular to characterize the
plane stress toughness of ductile polymers and related systems. The widespread use of the …
plane stress toughness of ductile polymers and related systems. The widespread use of the …
[HTML][HTML] Clay-based polymer nanocomposites: essential work of fracture
EA Franco-Urquiza - Polymers, 2021 - mdpi.com
This work details the general structure of the clays used as a reinforcement phase in
polymer nanocomposites. Clays are formed by the molecular arrangement of atomic planes …
polymer nanocomposites. Clays are formed by the molecular arrangement of atomic planes …
The essential work of fracture (EWF) method–analyzing the post-yielding fracture mechanics of polymers
AB Martinez, J Gamez-Perez, M Sanchez-Soto… - Engineering failure …, 2009 - Elsevier
The Post-Yielding Fracture Mechanics describe the fracture behaviour of pre-cracked films
and thin sheets that show yielding phenomenon at the crack tip during fracture. The …
and thin sheets that show yielding phenomenon at the crack tip during fracture. The …
The effect of weak interface on the fracture behavior of material extrusion 3D-printed polyetherimide
Y Zhang, H Ye, L Yuan, C Luo, X Ren, Q Yu… - Applied Materials …, 2023 - Elsevier
Understanding the mechanical response and toughening behavior of 3D printed high-
performance polymers, with regarding to the weak interface and undesirable internal voids …
performance polymers, with regarding to the weak interface and undesirable internal voids …
Fracture studies of polypropylene/nanoclay composite. Part I: Effect of loading rates on essential work of fracture
K Saminathan, P Selvakumar, N Bhatnagar - Polymer testing, 2008 - Elsevier
Polypropylene (PP)/Montmorillonite (MMT) nanoclay based composite was prepared by melt
compounding with maleic anhydride grafted polypropylene (MA-g-PP) as a compatibilizer in …
compounding with maleic anhydride grafted polypropylene (MA-g-PP) as a compatibilizer in …
The influence of nanosilica on the nucleation, crystallization and tensile properties of PP–PC and PP–PA blends
Immiscible blends of 80 wt% polypropylene (PP) with 20 wt% polyamide (PA) or
polycarbonate (PC) were prepared by melt mixing with or without the addition of 5 …
polycarbonate (PC) were prepared by melt mixing with or without the addition of 5 …
Does the length of the short chain branch affect the mechanical properties of linear low density polyethylenes? An investigation based on films of copolymers of …
P Gupta, GL Wilkes, AM Sukhadia, RK Krishnaswamy… - Polymer, 2005 - Elsevier
Three nearly identical linear low density polyethylene resins based on copolymers of
ethylene with 1-butene (B), 1-hexene (H) and 1-octene (O) were utilized to investigate the …
ethylene with 1-butene (B), 1-hexene (H) and 1-octene (O) were utilized to investigate the …
Essential work of fracture assessment of acrylonitrile butadiene styrene (ABS) processed via fused filament fabrication additive manufacturing
Experiments and finite element (FE) calculations were performed to study the raster angle–
dependent fracture behaviour of acrylonitrile butadiene styrene (ABS) thermoplastic …
dependent fracture behaviour of acrylonitrile butadiene styrene (ABS) thermoplastic …
The effect of rubber functionality on the phase morphology, mechanical performance and toughening mechanisms of highly toughened PP/PA6/EPDM ternary blends
M Hasanpour, MM Mazidi, MKR Aghjeh - Polymer Testing, 2019 - Elsevier
The main purpose of the present work was to study the phase morphology, mechanical
properties and fracture behavior of PP/PA6/(EPDM: EPDM-g-MA)(70/15/15) ternary blends …
properties and fracture behavior of PP/PA6/(EPDM: EPDM-g-MA)(70/15/15) ternary blends …
Temperature dependence of crack initiation fracture toughness of various nanoparticles filled polyamide 66
H Zhang, Z Zhang, JL Yang, K Friedrich - Polymer, 2006 - Elsevier
In the present study, the crack initiation fracture toughness of various nanoparticles filled
polyamide 66 was investigated in a broad temperature range (23–120° C) by using an …
polyamide 66 was investigated in a broad temperature range (23–120° C) by using an …