Effect of various phase fraction of bainite, intercritical ferrite, retained austenite and pearlite on the corrosion behavior of multiphase steels
PK Katiyar, S Sangal, K Mondal - Corrosion Science, 2021 - Elsevier
The work discusses the corrosion behavior of a set of newly developed high strength and
highly ductile multiphase steels consisting of various fractions of bainite, intercritical ferrite …
highly ductile multiphase steels consisting of various fractions of bainite, intercritical ferrite …
Evolution of crystal structure of Cu precipitates in a low carbon steel
Intercritical tempering at 680° C for different times was carried out in a low carbon copper-
bearing steel to study the evolution of the crystal structure of Cu precipitates by high …
bearing steel to study the evolution of the crystal structure of Cu precipitates by high …
Effects of austempering temperature on bainitic microstructure and mechanical properties of a high-C high-Si steel
J Zhao, B Lv, F Zhang, Z Yang, L Qian, C Chen… - Materials Science and …, 2019 - Elsevier
High tensile strength of~ 1550 MPa, uniform elongation of~ 30%, and impact energy of~ 80 J
were achieved in a high-C high-Si bainitic steel, by austempering around the nose-tip …
were achieved in a high-C high-Si bainitic steel, by austempering around the nose-tip …
A Review on Measurement Techniques of Deformation‐Induced Transformation Kinetics in Transformation‐Induced Plasticity and Transformation‐Induced Plasticity …
P Tiwari, A Varshney - steel research international, 2024 - Wiley Online Library
Deformation‐induced austenite‐to‐martensite transformation is an important phenomenon
that controls the flow behavior of transformation‐induced‐plasticity (TRIP) and TRIP …
that controls the flow behavior of transformation‐induced‐plasticity (TRIP) and TRIP …
A “new” empirical equation to describe the strain hardening behavior of steels and other metallic materials
The strain hardening behavior of five different steels of varying carbon content, ranging
between 0.007 and 0.71%, such as an Interstitial free (IF), a microalloyed, and a low …
between 0.007 and 0.71%, such as an Interstitial free (IF), a microalloyed, and a low …
Influence of microstructure on slurry erosion resistance of medium carbon high silicon steels
The present study compares slurry erosion resistance of austempered and tempered
medium carbon high silicon steels. A 0.62 C-1.91 Si-0.85 Mn-0.23 Cr steel was subjected to …
medium carbon high silicon steels. A 0.62 C-1.91 Si-0.85 Mn-0.23 Cr steel was subjected to …
Influence of quenching strategy on phase transformation and mechanical properties of low alloy steel
The energy-efficient quenching and nonisothermal partitioning process has been shown to
engender an excellent strength-ductility combination in low alloy steels. Conventionally …
engender an excellent strength-ductility combination in low alloy steels. Conventionally …
[HTML][HTML] Improvement of the fatigue crack growth resistance in AISI 4140 steel under single-and multi-austempering heat treatments
AISI 4140 steel under annealing conditions was subjected to single-and multi-austempering
heat treatments. The mechanical performance of the compact tension (CT) specimens was …
heat treatments. The mechanical performance of the compact tension (CT) specimens was …
On the extent of transformation of austenite to bainitic ferrite and carbide during austempering of high Si steel for prolonged duration and its effect on mechanical …
A Varshney, S Sangal, AK Pramanick… - Materials Science and …, 2020 - Elsevier
In this work, the effect of holding durations (10–60min) during austempering at 300, 350 and
400° C on the structure and properties of a 0.61 C-1.71 Si-0.86 Mn steel has been studied …
400° C on the structure and properties of a 0.61 C-1.71 Si-0.86 Mn steel has been studied …
Effect of austempering temperature on high cycle fatigue behaviour in nanostructured bainitic steels
The effect of three different austempering temperatures viz. 250° C (NB250), 300° C
(NB300) and 350° C (NB350) on high cycle fatigue behaviour of carbide-free nanostructured …
(NB300) and 350° C (NB350) on high cycle fatigue behaviour of carbide-free nanostructured …