Research advances in residual thermal stress of ceramic/metal brazes
Brazing, as a common method of bonding ceramic and metal, has been applied in
microelectronics, aerospace, machinery and other domains extensively. The residual …
microelectronics, aerospace, machinery and other domains extensively. The residual …
Brazing filler metals
M Way, J Willingham, R Goodall - International materials …, 2020 - journals.sagepub.com
Brazing is a 5000-year-old joining process which still meets advanced joining challenges
today. In brazing, components are joined by heating above the melting point of a filler metal …
today. In brazing, components are joined by heating above the melting point of a filler metal …
[HTML][HTML] A review paper on effect of the welding process of ceramics and metals
Y Zhang, YK Chen, DS Yu, DQ Sun, HM Li - Journal of Materials Research …, 2020 - Elsevier
As two important industrial manufacturing materials, ceramics and metals have their own
advantages and disadvantages in terms of physical, chemical, and mechanical properties …
advantages and disadvantages in terms of physical, chemical, and mechanical properties …
[HTML][HTML] Design and preparation of high-content Sc2W3O12 dispersed interlayer: alleviating the high residual stress of Cf/SiC and GH3536 joint
P Wang, J Li, W Liu, X Nai, S Zhao, H Chen… - Journal of Materials …, 2023 - Elsevier
Negative thermal expansion (NTE) materials were utilized to alleviate the high residual
stress of brazed joints by regulating the coefficient of thermal expansion (CTE) of metal …
stress of brazed joints by regulating the coefficient of thermal expansion (CTE) of metal …
Residual stress induced failure of Ti-6Al-4V/Si3N4 joints brazed with Ag-Cu-Ti filler: The effects of brazing zone's elasto-plasticity and ceramics' intrinsic properties
FS Ong, B Rheingans, K Goto, H Tobe… - Journal of the European …, 2021 - Elsevier
The residual-stress induced failure of Ti-6Al-4V/Si 3 N 4 joints brazed with two different Si 3
N 4 ceramics possessing different intrinsic properties was elucidated through experimental …
N 4 ceramics possessing different intrinsic properties was elucidated through experimental …
Friction stir vibration brazing (FSVB): an improved version of friction stir brazing
Friction stir vibration brazing (FSVB) by application of mechanical vibration was introduced
in this investigation. In the current research, the adjoining samples are vibrated normally to …
in this investigation. In the current research, the adjoining samples are vibrated normally to …
Interfacial microstructure and mechanical properties of ZrB2SiCC ceramic and GH99 superalloy joints brazed with a Ti-modified FeCoNiCrCu high-entropy alloy
A kind of novel composite filler was designed using FeCoNiCrCu high entropy alloy and
pure Ti foil. ZrB 2 single bondSiCsingle bondC ceramic and GH99 superalloy were brazed …
pure Ti foil. ZrB 2 single bondSiCsingle bondC ceramic and GH99 superalloy were brazed …
Constructing a heterogeneous interlayer in relieving the residual stresses for the AlN/Cu brazed joint used in IGBT
The aluminum nitride (AlN) ceramic is a underlying substrate material for high-voltage/power
insulated gate bipolar transistors (IGBT), due to its excellent thermal conductivity and low …
insulated gate bipolar transistors (IGBT), due to its excellent thermal conductivity and low …
Brazing SiC ceramic using novel B4C reinforced Ag–Cu–Ti composite filler
X Dai, J Cao, Z Chen, X Song, J Feng - Ceramics International, 2016 - Elsevier
The development of new composite fillers is crucial for joining ceramics or ceramics to
metals because the composite fillers exhibit more advantages than traditional brazing filler …
metals because the composite fillers exhibit more advantages than traditional brazing filler …
Reactive brazing of silicon nitride to Invar alloy using Ni foam and AgCuTi intermediate layers
W Guo, H Zhang, K Ma, Y Zhu, H Zhang, B Qi, F Li… - Ceramics …, 2019 - Elsevier
Abstract Silicon nitride (Si 3 N 4) ceramic and Invar alloy have been brazed by using AgCuTi
active filler and the Ni foam was added to further improve mechanical properties of joints in …
active filler and the Ni foam was added to further improve mechanical properties of joints in …