High temperature materials for heavy duty diesel engines: Historical and future trends

D Pierce, A Haynes, J Hughes, R Graves… - Progress in Materials …, 2019 - Elsevier
Heavy duty (HD) vehicles are projected to be the largest fuel-use subsector in transportation,
with current demand for diesel fuel projected to grow 30% by 2040. Historically, a primary …

Invited Review Paper in Commemoration of Over 50 Years of Oxidation of Metals: Addressing the Role of Water Vapor on Long-Term Stainless Steel Oxidation …

BA Pint - Oxidation of Metals, 2021 - Springer
In the past 20 years, it has become clear that the long-term exposure of chromia-forming
austenitic stainless steels to air containing~ 10 vol% water vapor at 650–800° C significantly …

The braking performance and failure mechanism of copper-based brake pads during repeated emergency braking at 400 km/h

P Zhang, D Wei, E Mei, B **e, Y Liang, X Ding, L Zhang… - Wear, 2024 - Elsevier
Copper-based brake pads have played a pivotal role in the braking systems of commercial
high-speed trains travelling at speeds ranging from 200 to 350 km/h. In this study, the …

Long-term oxidation of candidate cast iron and stainless steel exhaust system alloys from 650 to 800 C in air with water vapor

MP Brady, G Muralidharan, DN Leonard, JA Haynes… - Oxidation of metals, 2014 - Springer
The oxidation behavior of candidate cast irons and cast stainless steels for diesel exhaust
systems was studied for 5,000 h at 650–800° C in air with 10% H 2 O. At 650° C, Ni-resist …

Improving the high-temperature oxidation resistance of ASME-SA213-T11 boiler tube steel by plasma spraying with CNT-reinforced alumina coatings

R Goyal, BS Sidhu, V Chawla - Anti-Corrosion Methods and Materials, 2018 - emerald.com
Purpose This paper aims to discuss that a conventional Al2O3, 1.5 Wt.% carbon nanotubes
(CNTs)-Al2O3, 2 Wt.% CNTs-Al2O3 and 4 Wt.% CNTs-Al2O3 composite coatings were …

Morphologies of oxide growth and exfoliation in superheater and reheater tubing of steam boiler

IG Wright, R Barry Dooley - Materials at High Temperatures, 2011 - Taylor & Francis
The intent of this paper is to present the current state of knowledge concerning the
development of the oxide morphologies associated with scales grown in steam on alloys …

The effect of shot peening on steam oxidation of 304H stainless steel

JM Kurley, BA Pint - Oxidation of Metals, 2020 - Springer
Shot peening is currently utilized in coal-fired power plant components to mitigate scale
exfoliation issues from steamside oxidation of austenitic stainless steel superheater and …

Negative impact of thermal loads on pressure and non-pressure boiler parts

P Duda, Ł Felkowski - Energies, 2023 - mdpi.com
Issues related to the proper design of power boiler elements taking account of thermal loads
are still relevant in this era of increasing variability of the boiler power output over time. The …

Phase-field modeling of crack growth and mitigation in solid oxide cells

F Xue, Y Lei, TL Cheng, WK Epting, G Hackett… - International Journal of …, 2023 - Elsevier
Fracture and crack growth is one of the main degradation mechanisms in solid oxide cells
(SOCs). However, the modeling of crack growth in SOCs is challenging due to their complex …

Oxide scale exfoliation and regrowth in TP347H superheater tubes

AS Sabau, IG Wright… - Materials and …, 2012 - Wiley Online Library
This paper provides an introduction to a comprehensive model being developed to predict
and control oxide scale exfoliation from the steam‐side of superheater and reheater tubes in …