Turnitin
降AI改写
早检测系统
早降重系统
Turnitin-UK版
万方检测-期刊版
维普编辑部版
Grammarly检测
Paperpass检测
checkpass检测
PaperYY检测
Microstructural stability of cemented carbides at high temperatures: Modeling the effect on the hot hardness
V Lamelas, MB Rolland, M Walbrühl… - International Journal of …, 2024 - Elsevier
There are several semi-empirical models available in literature that correlate the intrinsic
hardness of cemented carbides' constitutive phases and certain microstructural parameters …
hardness of cemented carbides' constitutive phases and certain microstructural parameters …
Room-temperature deformation of single crystals of WC investigated by micropillar compression
K Kishida, M Morisaki, M Ito, Z Wang, H Inui - Acta Materialia, 2023 - Elsevier
The room temperature deformation behavior of single crystals of WC has been investigated
as a function of crystal orientation and specimen size by micropillar compression tests …
as a function of crystal orientation and specimen size by micropillar compression tests …
Improved electrochemical and mechanical performance of WC-Co cemented carbide by replacing a part of Co with Al2O3
In this study, WC/xCo/6-xAl 2 O 3 (x= 1, 2, 3 and 6 wt%) composites were fabricated through
spark plasma sintering. The electrochemical and mechanical properties of the composites …
spark plasma sintering. The electrochemical and mechanical properties of the composites …
Vacuum brazed Ni-based coating reinforced with core-shell WC@ Cu/Co-P
Improving the wettability and bond strength of WC with Ni-based matrix and preventing the
growth of WC in the melt of Ni-based alloy are always the challenges that should be …
growth of WC in the melt of Ni-based alloy are always the challenges that should be …
Void formation driven by plastic strain partitioning during creep deformation of WC-Co
L Weller, R M'saoubi, F Giuliani… - International Journal of …, 2024 - Elsevier
Creep deformation of WC-Co composites at high temperature and stress is accommodated
by either bulk WC phase creep deformation or by Co-infiltrated grain boundary sliding. It has …
by either bulk WC phase creep deformation or by Co-infiltrated grain boundary sliding. It has …
A comprehensive constitutive equation for the hot deformation of WC-Co
Hot deformation of five microstructurally different sintered WC-Co cemented carbides during
hot compression testing was investigated in the temperature range of 700–1000° C and at …
hot compression testing was investigated in the temperature range of 700–1000° C and at …
An observation of the binder microstructure in WC-(Co+ Ru) cemented carbides using transmission Kikuchi diffraction
The microstructure of WC-(Co+ Ru) cemented carbides was studied using transmission
Kikuchi diffraction (TKD). We report that the Co FCC grains contain Σ3-annealing twins …
Kikuchi diffraction (TKD). We report that the Co FCC grains contain Σ3-annealing twins …
Micropillar compression of single crystal tungsten carbide, Part 1: Temperature and orientation dependence of deformation behaviour
Tungsten carbide cobalt hardmetals are commonly used as cutting tools subject to high
operation temperature and pressures, where the mechanical performance of the tungsten …
operation temperature and pressures, where the mechanical performance of the tungsten …
Creep behaviour of WC-12 wt% Co hardmetals with different WC grain sizes tested in uniaxial tensile and compression step-loading tests at 700° C and 800° C
K Maier, T Klünsner, M Krobath, P Pichler… - International Journal of …, 2021 - Elsevier
At elevated temperatures, the material behaviour of WC-Co hardmetals shows differences
under similar loading conditions depending on WC grain size and Co-content. Variations in …
under similar loading conditions depending on WC grain size and Co-content. Variations in …
Improved electrochemical corrosion resistance of hot-press sintered WC–Al2O3 composites with added TiC in alkaline solutions
B Han, S Zhu, W Dong, Y Bai, H Ding, Y Luo, P Di - Ceramics International, 2021 - Elsevier
x) WC–15 wt% Al 2 O 3–xTiC (x= 0, 1.5, 2.5, 5, 10, and 20 wt%) composites were prepared
by vacuum hot-press sintering. The influence of TiC addition on the corrosion behaviour of …
by vacuum hot-press sintering. The influence of TiC addition on the corrosion behaviour of …